What is the point of using a solvent free product?
No buzz - no joy!!
No need to polish the last layer. I used the marine varnish undiluted for maybe 4 layers, with a flattening with Wet and Dry paper after each coat. This way I achieved a perfectly flat surface, masking all undulations and irregularities in the wood panels.
For the last layer I diluted the laquer to thin it, and sieved it through a fine cloth to get rid of the little lumps.
It does not matter hich product you use, you need several layers. The thicker layer - the better "depth".
I forgot: If the veneer is cracked, it is usually better to give the job to a pro.
No need to go to a person that does cars, I would go to a person that does furniture restorations.
The same if I wanted to re-veneer the dashboard or the other bits.
In 1992 I veneered the dashboard and gearshift fascia on my 1991 AR Spider S4. I hated the crappy black plastic.
I used a veneer from the root section of Mahogany (proper Rainforest stuff in those days).
Lokked perfect untill I sold the car in 2004.
Marine varnish can take some water.